The temper of 7075 aluminum extrusions can be T6, T6510, T6511, T73, T73510, T73511, T76, T76510, T76511.
| Temper | Description |
|---|---|
| T6 | solution heat treated, artificially aged. |
| T6510 | solution heat treated, stress-relieved by stretching, artificially aged with no hard straightening. |
| T6511 | solution heat treated, stress-relieved by stretching, artificially aged with minor straightening. |
| T73 | solution heat treated, artificially overaged to achieve best stress corrosion resistance. |
| T73510 | solution heat treated, stress-relieved by stretching, artificially overaged to achieve best stress corrosion resistance with no hard straightening. |
| T73511 | solution heat treated, stress-relieved by stretching, artificially overaged to achieve best stress corrosion resistance with minor straightening. |
| T76 | solution heat treated, artificially overaged to achieve good exfoliation resistance. |
| T76510 | solution heat treated, stress-relieved by stretching, artificially overaged to achieve good exfoliation resistance with no hard straightening. |
| T76511 | solution heat treated, stress-relieved by stretching, artificially overaged to achieve good exfoliation resistance with minor straightening. |